Mortar Calculator β Bags for Any Masonry Project
Reviewed and updated: August 2026
Calculate bags of mortar mix for brick walls, CMU block, and stone projects. Covers Type S, Type N, and Type M mortar with joint size adjustments.
ft
ft
ft
ft
sq ft
%
$
YOUR RESULTS
60 lb Bags
β
bags
80 lb Bags
β
bags
Mortar Volume
β
cu ft
Mortar Type
β
Material Cost
β
est.
Mortar Type Guide
Type
Strength
Best Use
Type S
1,800 psi
Exterior walls, below grade, pavers
Type N
750 psi
Interior walls, above-grade non-structural
Type M
2,500 psi
Foundations, retaining walls, driveways
Choose your masonry type (brick, CMU block, or stone), enter the wall dimensions and joint thickness, select your mortar type, and get the number of 60 lb and 80 lb bags needed along with total mortar volume and cost. A 15% waste factor is built in by default: mortar is inexpensive but running out mid-course creates weak cold joints that are nearly impossible to repair invisibly.
How to Calculate Mortar Needed
Mortar volume is determined by the number and size of joints in your wall. For brick, every course has a bed joint (horizontal) and head joints (vertical ends). The more joints per square foot: which increases with smaller bricks and larger joint widths: the more mortar required.
Worked example: a 20Γ4 ft brick wall (80 sq ft) using standard bricks at 3/8" joints. The wall has about 540 bricks (80 Γ 6.75). At 27 bricks per 60 lb bag of mortar at this joint size, that's 20 bags base, add 15% waste = 23 bags. At $12 per bag, mortar cost is about $276 for this wall section.
Bed Joints and Head Joints, Visualized
Every brick or block in a wall is surrounded by mortar on two types of joints: the horizontal bed joint it sits on, and the vertical head joints on either side. Both consume mortar, which is why joint count, not just wall area, drives total volume.
Mortar Type Comparison
Type
Compressive Strength
Flexibility
Primary Use
Site Mix Ratio
Type M
2,500 psi
Lowest
Foundations, heavy retaining walls, below grade
1 cement : ΒΌ lime : 3 sand
Type S
1,800 psi
Moderate
Exterior masonry, pavers, most structural work
1 cement : Β½ lime : 4.5 sand
Type N
750 psi
Higher
Interior non-load-bearing, repointing soft brick
1 cement : 1 lime : 6 sand
Type O
350 psi
Highest
Interior non-structural, historic preservation
1 cement : 2 lime : 9 sand
Mortar Coverage Reference
Application
Joint Size
60 lb Bag Coverage
Notes
Standard brick wall
3/8"
~25β30 bricks
Bed + head joints combined
Standard CMU block
3/8"
~10β12 blocks
Face-shell bedding (hollow cores not filled)
Fieldstone / rubble
3/4"β1"
~8β12 sq ft
Wide irregular joints use significantly more mortar
Ashlar / cut stone
1/2"β3/4"
~15β20 sq ft
Tighter joints, more predictable coverage
Paver bedding (Type S)
3/8" joints
~30β40 sq ft
Thin-set style application
Mortar Joint Tooling Styles
How a joint is finished (tooled) after the mortar has begun to set affects both appearance and water resistance, which is why it matters beyond aesthetics:
Joint Style
Weather Resistance
Common Use
Concave (most common)
Excellent
Standard residential brick and block
V-joint
Excellent
Similar performance to concave; sharper shadow line
Flush
Good
Modern aesthetic; less pronounced shadow lines
Struck
Poor
Historic look; ledge collects water, not recommended for exterior
Raked
Poor
Deep shadow lines; recessed joint traps moisture
Concave and V-joints compress the mortar surface as they're tooled, which closes surface pores and sheds water effectively. Struck and raked joints leave a ledge or recess that can hold water against the masonry, accelerating freeze-thaw damage in cold climates. For any exterior wall in a climate with freezing winters, concave or V-joint tooling is the safer long-term choice regardless of the aesthetic preference.
Pre-Mix vs. Site-Mixed Mortar
Pre-mix mortar bags (just add water) are ideal for projects under 10 bags: no measuring, no separate purchases. For larger jobs, site-mixing cement, lime, and masonry sand separately is more economical, typically 30β40% cheaper per cubic foot of mortar. The standard Type S site-mix ratio is 1 part Portland cement : Β½ part hydrated lime : 4.5 parts masonry sand, measured by volume.
Mortar Curing Guide
Stage
Time
What to Do
Initial set
1β2 hours
Tool joints (strike when thumbprint-firm)
Walk-on strength
24 hours
Light foot traffic on pavers acceptable
50% strength
24β48 hours
Keep moist: mist 2β3Γ daily in heat
Full cure
28 days
Full design strength achieved
Cold weather (<40Β°F)
N/A
Use cold-weather additives or stop work; mortar will not cure below freezing
Common Mortar Mistakes
Using Type N mortar below grade or on exterior retaining walls. Type N lacks the compressive strength and moisture resistance for these applications. Any masonry that contacts soil, sits below the frost line, or is exposed to freeze-thaw cycles requires Type S or Type M.
Mixing mortar too wet. Mortar should have a "peanut butter" consistency: it holds its shape when scooped but spreads smoothly with a trowel. Wet mortar shrinks more as it cures, weakening the bond and increasing the risk of cracking. Never add more water once the mix has started to stiffen.
Letting mortar stiffen before placing the masonry unit. Mortar that has started to set (>2 hours in normal conditions) must be discarded: never re-tempered with water and reused. A cold joint formed by placing brick on stiffened mortar is mechanically weak and won't pass inspection.
Skipping the misting cure on hot or windy days. In temperatures above 90Β°F or with strong wind, mortar loses moisture too quickly and never achieves full strength. Keep fresh mortar joints moist for the first 24β48 hours using a fine mist: this is especially important for exterior work in summer.
Using the same mortar mix for repointing as for new work. Repointing (tuckpointing) old brick walls should use a mortar no stronger than the original: often Type N or even Type O for pre-1940s soft brick. A rigid Type S mortar in an old soft-brick wall will cause the bricks to spall as the mortar is stronger than the brick face.
Site tip: Mix only as much mortar as you can use in 1β2 hours. In hot weather, reduce that to 45 minutes. Keep your mixing water cool and work in the shade when possible. Stiffening mortar cannot be revived by adding water: the chemical set has begun and re-tempering destroys the bond strength. Smaller, more frequent batches always produce better results than one large batch that partly stiffens.
A 60 lb bag of mortar mix covers approximately 25β30 standard bricks with 3/8" joints. An 80 lb bag covers about 35β40 bricks. These numbers assume normal mason technique with both bed and head joints. Wider joints (1/2") reduce coverage to 20β25 bricks per 60 lb bag; narrower joints (1/4") increase it to 35+ bricks. Always add 15% to your mortar estimate for spillage and waste.
What is the difference between mortar and grout? βΎ
Mortar is a thick paste used to bed and join masonry units (brick, block, stone): it's applied with a trowel and stays in the joints. Grout is a thinner, poured mixture used to fill cavities inside CMU block cores and, separately, the joints between ceramic or porcelain tiles. For tile work, use our tile calculator which accounts for both thinset adhesive mortar and grout joints separately.
How long does mortar take to cure? βΎ
Mortar begins to set within 1β2 hours and reaches about 50% strength in 24β48 hours. Full cure takes 28 days, similar to concrete. Keep fresh mortar moist for the first 24β48 hours in hot, dry, or windy conditions by misting with water 2β3 times daily. Never apply mortar below 40Β°F: it will not cure properly and will fail. In cold weather, use heated enclosures or cold-weather mortar additives per manufacturer instructions.
Can I mix my own mortar instead of buying bags? βΎ
Yes: for large projects, site-mixing is typically 30β40% cheaper than pre-mixed bags. The standard Type S mix is 1 part Portland cement : Β½ part hydrated lime : 4Β½ parts masonry sand, measured by volume. Use clean masonry sand (not beach or play sand), and mix dry ingredients before adding water gradually until you reach a smooth, peanut-butter consistency. For projects under 10 bags, pre-mix bags are more convenient and eliminate measuring errors.
What mortar should I use for repointing old brick? βΎ
Use a mortar no stronger than the original: typically Type N (750 psi) or Type O (350 psi) for pre-1950s brick. Modern Type S mortar (1,800 psi) is harder than many historic brick faces. When a wall expands and contracts seasonally, the weakest material should fail: in a properly designed wall, that's the mortar joint (which is repairable), not the brick face (which is not). Using too-strong mortar in old brick causes spalling and permanent brick damage. Test the original mortar hardness with a key scratch: if it scratches easily, use Type N or O for repointing.